Shchekina N.A.

Postgraduate, Belgorod State Technological University named after V.G. Shukhov, Russia

Experimental studies of the processes of structure formation of composite mixtures with technogenic mechanoactivated silica component

https://doi.org/10.58224/2618-7183-2023-6-2-5-18
Abstract
The paper considers the issues of utilization of technogenic fibrous material – waste of basalt production. The chemical composition of the technogenic fibrous material was studied, it was found that it consists of 44% SiO2. The initial basalt rock, which undergoes changes during high-temperature processing in the process of obtaining basalt fiber, was studied using IR spectroscopy. The grinding of the crowns was carried out for 30 minutes, allowing to reach a specific surface area of 800 m2 / kg. Further grinding does not lead to an increase in the specific surface area, which is associated with the phenomenon of secondary aggregation of fine particles. Research on REM has shown that the “cold shots” before grinding are mostly rounded or oval in shape. The compositions were formed and the strength characteristics of the samples for the 3rd and 28th day were determined. The maximum strength gain of 59 MPa was established at the age of 28 days in samples with the addition of 5% ground “cold shots” . When introducing cold shots in an amount of 10% (composition 5) of the cement mass, an intensive strength gain is noted in the early stages of hardening (7 days) with a strength of 38 MPa, slightly higher than the strength of the control composition. The introduction of 15% ground “cold shots” gives a strength value slightly lower (32 MPa) than the values of the control composition (37 MPa) at all stages of hardening.
PDF

THE RELIABILITY COEFFICIENT FOR FIBRE CONCRETE MATERIAL

https://doi.org/10.58224/2618-7183-2022-5-2-51-58
Abstract
One of the main parameters of the method for calculating building structures made of concrete and fibre concrete by limiting states is the reliability coefficient for the material, which characterizes the heterogeneity of the physical and mechanical properties of the material. In national and foreign standards, it takes a constant value of 1.3 (obtained on the basis of direct tests), or 1.5 (obtained on the basis of indirect tests and the use of graduated dependencies). The concrete matrix for the formation of the structure of fibre concrete is most often fine-grained concrete with special additives, which has greater uniformity in comparison with heavy concrete, which cannot but affect the reliability of the composite material in question as a whole: the stock coefficients for fibre concrete should be lower than for normal concrete, which has not been reflected in modern standards for design yet. Starting from interval estimates of the average strength value, a new approach to determining the reliability coefficient for the material, differentiated by the 1st and 2nd groups of limit states, is proposed. The results of calculations according to the proposed formulas for previously conducted tests of steel- and glass-fiber concrete images allowed us to conclude: the introduction of fiber into the concrete matrix of the proposed effective composite composition increases the uniformity of the strength properties of the material, which leads to an increase in the reliability of its use in building structures, a decrease in the value of the reliability coefficient (margin) for the material to 1.164...1.235 for central axial compression and up to 1.172...1.272 – for central axial stretching. The obtained actual coefficients in strength calculations will allow to reveal the supplemented reserves of the bearing capacity of structures made of this material up to 22.4%.
PDF